ZnO-CdO (Zinc cadmium oxide, ZnCdO)

Glasses, oxides and dielectrics

8 datasets, together covering 0.3–3.2 µm. Default: Aguilar et al. 2019: n,k 0.3–3.2 µm; 10% ZnO.

Use it in Lightsmith

Load this data in Python, simulate in one more line

pip install lightsmith
import lightsmith as ls

# ZnO-CdO (Zinc cadmium oxide, ZnCdO): Aguilar et al. 2019: n,k 0.3–3.2 µm; 10% ZnO
zno_cdo = ls.fetch_refractiveindex("other", "ZnO-CdO", "Aguilar-10", ref="c5c2f188e848453def5970e347399d653df2ffc2")
print(zno_cdo.range_nm)  # (300, 3200) nm
eps = zno_cdo.eps([633])  # complex permittivity

Downloads the original record once (pinned to the imported snapshot) and caches it.

Lightsmith is open source (MIT): Mie, T-matrix, BEM, DDA, FDTD, RCWA, TMM, mode solvers and inverse design behind one spec, on CPU or GPU. GitHub.

About ZnO-CdO (Zinc cadmium oxide, ZnCdO)

Other names: Zinc cadmium oxide, ZnCdO, Zinc-cadmium oxide, ZnCdO

API: /v1/materials/mat_203009332e94 · slug zno-cdo